ITS TEST REPORT N120047534-231-01 IMPACT TESTING <br /> MODEL:ORGANIC COATED GLASS <br /> CLIENT:COMMONWEALTH LAMINATING&COATING <br /> TEST DATE:JULY 20-24,2001 Page 4 of4 <br /> Results Continued: <br /> 8mil <br /> Impact Distance at <br /> Which <br /> Disintegration <br /> Specimen Test Occurred; <br /> # Standard Inches Results Allowed <br /> I' ANSI 297.I 18 Sample broke No shear or opening <br /> no opening created >3"diameter <br /> 2* ANSI Z97,I 18 Sample broke No shear or opening <br /> no opening created >3"diameter <br /> 34 CPSC 1201 18 Sample broke No shear or opening <br /> no opening created >3"diameter <br /> 4** ANSI Z97.I 12 Sample broke No shear or opening <br /> no opening created >3"diameter <br /> 5** ANSI Z97.2 18 Sample broke No shear or opening <br /> no opening created >3"diameter <br /> 6** CPSC 1201 48 Sample broke No shear or opening <br /> no opening created >3"diameter <br /> *Impacted laminated side <br /> **Impacted non-laminated side <br /> CONCLUSIONS <br /> The 4 mil, 7 mil,and 8 mil organic coated glass samples wider evaluation,satisfactorily meet the <br /> safety requirements of ANSI Z97.1 and CPSC 16 CRF 1201 impact test due to the fact that the <br /> samples broke with out creating sheer or opening that allowed a three-inch sphere to pass. <br /> The 4 mil, 7 mil,and 8 mil qualify for category, I(one)classification per CPSC 16 CRF 1201 <br /> Test Conducted by: Report Reviewed by: <br /> rw �-- <br /> Jesse Grossbier ryfi Turgeson <br /> Engineering Technician }enestration Manager <br /> `r <br /> £'d 6068699E09 sweipHM cep d98:A 60 01 des <br />